Q
Snake-like curved lines appear on the product from the gate
A
Jetting requires reducing the initial injection speed and adjusting the gate
Extrusion & Post jettingsnake-like linesgateinjection speed
Q
Differences in molecular weight, additive content, etc. between batches affect processing stability
A
Batch differences require incoming inspection and parameter fine-tuning
Material Drying batch differencemolecular weightadditiveincoming inspection
Q
Low-temperature performance changes of PA-type materials require evaluation of applicability
A
PA at low temperature requires impact testing and selection of suitable grades
Material Drying low-temperature performancePA brittlenessimpact testPA12
Q
Equipment parameters not matching material characteristics affect processing quality
A
Equipment needs to match cellulose acetate butyrate characteristics and product requirements
Injection Molding equipment selectionclamping forcescrewtemperature control
Q
Compression molding is used to reduce warpage and internal stress but the parameters are set improperly
A
Compression molding requires precise timing and force control
Injection Molding compression moldingcompression timingwarpage reductioncellulose acetate butyrate
Q
Unreasonable temperature settings in each zone affect plasticization and extrusion quality
A
Extrusion temperature needs to be reasonably set for each zone according to the gradient
Extrusion & Post extrusion temperaturezone controlgradientplasticization
Q
Mold temperature differences in different areas affect product quality
A
Mold temperature gradient needs to be set according to area and material characteristics
Molds & Tooling mold temperature gradientregional temperature differencecrystallizationPA
Q
Rear zone temperature deviating from the recommended value affects plasticization
A
Rear zone temperature needs to be set according to the gradient to ensure continuous plasticization
Molding Process rear zone temperatureplasticizationtemperature control gradient
Q
Improper annealing treatment, residual stress not eliminated or product deformed
A
Annealing requires slow cooling below the heat deflection temperature
Extrusion & Post annealingresidual stressheat deflection temperature
Q
Large shrinkage difference between the melt flow direction and the perpendicular direction
A
Orientation warpage requires reducing orientation and promoting relaxation
Injection Molding orientation warpageanisotropymolecular orientationannealing