Q
Melt Fracture in PU Extrusion
Q
Difficult Demolding in PU '2079851475616104452
A
Demolding difficulty is caused by adhesion and insufficient mold design; increasing draft angle is the fundamental measure
Injection Molding PU injectiondemolding difficultydraft angleadhesionejection design
Q
Bubbles in PU Injection Molded Thick-Walled Products
A
Thick-wall bubbles are caused by a combination of insufficient holding, moisture and poor venting
Material Drying PU injectionbubbleholding pressurethick-walled productmold venting
Q
EVOH Product Elliptical Deformation
A
Elliptical deformation is caused by asymmetric demolding force; uniform ejection is key
Molds & Tooling EVOHelliptical deformationsymmetric ejectionuniform coolingsetting time
Q
EVOH Surface Snakeskin Pattern
A
Snakeskin pattern is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed are key
Extrusion & Post EVOHsnakeskin patternextrusion temperatureelastic recoverydie temperature control
Q
EVOH Internal Delamination Cracking
A
Internal delamination is caused by poor interface and shrinkage differences; compatibilizer and uniform cooling are key
Extrusion & Post EVOHinternal delaminationinterfacial adhesioncompatibilizeruniform cooling
Q
EVOH Product Twist Deformation
A
Twist deformation is caused by asymmetric cooling; symmetric cooling is key
Molds & Tooling EVOHtwist deformationsymmetric coolinggate arrangementannealing
Q
Carbonized Black Specks Inside EVOH
A
Black specks are caused by thermal carbonization and carbon deposit; cooling and regular cleaning are key
Processing Machinery EVOHinternal black speckthermal carbonizationscrew cleaningtemperature control
Q
EVOH Flexural Modulus Too Low
A
Low flexural modulus is caused by material softness and insufficient filler; adding rigid filler is key
Material Analysis EVOHflexural modulusrigid fillernucleating agentcrystallinity
Q
Periodic EVOH Surface Ripples
A
Ripples are caused by unstable injection; equipment overhaul and PID control are key
Injection Molding EVOHsurface rippleinjection stabilityequipment overhaulPID control