Poor ABS demolding (mold sticking)

Sorun Belirtisi
The product adheres to the cavity or core, and is pulled injured, ejected white, or even punctured during demolding.
Neden Analizi
Too high holding pressure and too high melt/mold temperature make the product's gripping force large; insufficient draft angle; poor cavity polishing or roughening; vacuum adsorption effect.
Çözüm
①Reduce holding pressure and melt temperature; ②ensure a draft angle of 1°~3°; ③polish the cavity to repair pull injuries; ④fully cool before mold opening; ⑤add venting to avoid vacuum adsorption.
Temel Çıkarım
For mold sticking, first reduce pressure and temperature, then check the draft angle and polishing.
ABS;mold sticking;draft angle;gripping force;polishing