Molds & Tooling
8 görüntüleme
ABS uneven gloss
Sorun Belirtisi
ABS uneven gloss due to mold temperature fluctuation, inconsistent contact between resin and steel, temperature stabilization.
Neden Analizi
ABS uneven gloss; mold temperature fluctuation; inconsistent contact between resin and steel; surface quality; temperature controller stability; maintain 60-80℃.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Çözüm
①Stable mold temperature 60-80℃; ②temperature controller calibration; ③surface contact; ④gloss inspection; ⑤process stability.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
Mold temperature stability is the core for ABS uneven gloss; controller calibration ensures accuracy; inspection ensures consistency.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!