Molds & Tooling
8 görüntüleme
ASA uneven haze
Sorun Belirtisi
ASA product surface haze distribution is uneven, locally foggy and locally bright, differences obvious between different areas in the same cavity, appearance judgment controversial.
Neden Analizi
Surface haze is related to the slip state of the melt on the mold wall and shear history; uneven mold temperature, local shear difference and poor venting all cause surface microstructure differences, appearing as uneven haze.
Çözüm
①Balance mold temperature distribution to eliminate local temperature difference; ②stabilize injection speed curve to reduce shear fluctuation; ③improve venting; ④unify cavity surface treatment grade.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
The governance of ASA uneven haze returns to temperature and shear uniformity; appearance judgment standard should quantify haze value; cavity surface consistency is the basic guarantee.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!