Material Drying 5 görüntüleme

LCP Product Bubbles

Sorun Belirtisi
Bubbles inside the product.
Neden Analizi
Moisture on the pellet surface vaporizes or degradation generates gas; at high temperatures, moisture is the main source.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience
Çözüm
①Fully dry to below 0.01%; ②control melt temperature upper limit; ③shorten residence time; ④improve venting.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
LCP bubbles are mainly of the moisture type; strict drying solves the vast majority.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
LCP;bubble;moisture;drying;degradation;venting