Processing Machinery 5 görüntüleme

LDPE Film Air Volume and Pressure Setting

Sorun Belirtisi
The bubble is under-cooled or trembling; it improves after adjusting air volume and pressure to the recommended range.
Neden Analizi
Air volume and pressure deviate from the empirical ranges of 60~80% and 0.3~0.6MPa; improper air ring position relative to the die also affects cooling efficiency.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Çözüm
①Set air volume at 60~80% and air pressure at 0.3~0.6MPa; ②Fine-tune the air ring position 50~100mm from the die; ③Observe bubble shape for verification; ④Record the optimal settings.
Temel Çıkarım
Air volume and pressure have mature empirical ranges; fine-tuning based on them can quickly stabilize the bubble.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
LDPE; film; air volume; air pressure; air ring; cooling

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI