Extrusion & Post
5 görüntüleme
LLDPE film pinholes
Sorun Belirtisi
Tiny pinholes appear on the film surface, becoming barrier defects after lamination.
Neden Analizi
Gel rupture, bubbles, or impurity points form pinholes under high stretching; LLDPE high draw ratio applications expose them more easily.; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience.
Çözüm
①Strengthen filtration to reduce gel; ②control raw '2079851475616104451; ③visual inspection positioning; ④optimize the stretching process.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Temel Çıkarım
Pinholes are a quality red line for high-stretch film; source cleanliness and filtration are key.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!