Extrusion & Post 2 Aufrufe

LLDPE film pinholes

Problembeschreibung
Tiny pinholes appear on the film surface, becoming barrier defects after lamination.
Ursachenanalyse
Gel rupture, bubbles, or impurity points form pinholes under high stretching; LLDPE high draw ratio applications expose them more easily.; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience.
Lösung
①Strengthen filtration to reduce gel; ②control raw '2079851475616104451; ③visual inspection positioning; ④optimize the stretching process.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Wichtigste Erkenntnis
Pinholes are a quality red line for high-stretch film; source cleanliness and filtration are key.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
LLDPE; film; pinhole; gel; filtration; stretching