PA66 ejector whitening and cracking
Sorun Belirtisi
White marks and cracks at ejector pins, high incidence in deep-cavity parts.
Neden Analizi
Large gripping force + concentrated stress; insufficient cooling; PA66 has high rigidity and large gripping force; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience.
Çözüm
①Extend cooling time so products are fully set before demolding; ②increase ejector pin number and area or switch to a stripper plate to distribute ejection force; ③appropriately reduce holding pressure to reduce gripping force and frozen internal stress; ④polish the cavity or die lip to reduce surface resistance and improve replication; ⑤optimize ejector pin layout.
Temel Çıkarım
PA66 ejector whitening='concentrated stress': distribute ejection force and give sufficient cooling; high-rigidity nylon ejection systems must leave sufficient margin; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!