Menü
Malzemeler Makineler
İçgörüler
Makaleler Videolar Sorun ve Çözüm
About
Chembull Hakkında Medya Ortakları
Bize Ulaşın
Dil
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Sorun ve Çözüme Geri Dön
Molds & Tooling 4 görüntüleme

PCABS Venting Silver Streaks

Sorun Belirtisi
[Problem Phenomenon] PC/ABS silver streaks are concentrated at the product ends and ribs, with a regular distribution
Neden Analizi
Poor venting type silver streaks: gas is trapped at the parting line, ends, and ribs, and the gas cannot be discharged and is pressed on the surface layer to form silver streaks; often accompanied by burning; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Çözüm
Open venting grooves of 0.03-0.05mm at ends and ribs; add venting inserts in deep cavities; reduce end-stage injection speed to let gas out; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Temel Çıkarım
For venting silver streaks, watch the ends and ribs, with venting grooves of 0.03-0.05mm; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
venting silver streakstrapped gasventing grooveend

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI