PMMA Light Guide Plate Warpage
Sorun Belirtisi
Thin-wall light guide plates warp after demolding, dot replication is incomplete, and light leakage is uneven after assembly.
Neden Analizi
Thin-wall long-flow-path filling requires high pressure and creates large internal stress; uneven mold temperature and improper holding pressure cause inconsistent shrinkage, making optical-grade flatness hard to guarantee.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based on experience alone.
Çözüm
①Improve mold temperature uniformity; ②optimize holding pressure profile; ③multi-point gates for balanced filling; ④anneal to reduce stress.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Temel Çıkarım
Light guide plates are a high-difficulty category of PMMA '2079851475616104452; stress and flatness control is the core, and process and mold need synchronized fine design.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.