Molds & Tooling 5 görüntüleme

POM mold temperature 80-100°C

Sorun Belirtisi
Product surface shows ripples and wrinkles, obvious weld lines, or demolding burns and overly long cycles
Neden Analizi
POM cools and solidifies quickly; when the mold temperature is low, the surface layer quenches, producing ripples, marks, and weld lines; a mold temperature of 80-100°C can improve surface quality, and thin-walled long-flow complex parts can be raised to 120°C
Çözüm
①Routine mold temperature 80-100°C with hot oil circulation; ②raise to 120°C for thin-walled long-flow complex parts; ③use a mold temperature controller for precise control of precision products; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
Mold temperature is the first variable for POM surface quality; the 80-100°C baseline plus on-demand increases compensates for the shortcoming of fast cooling with mold temperature; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
POM;mold temperature;80-100°C;ripples;fast cooling