Molds & Tooling 8 görüntüleme

PPO Pin Gate Blockage

Sorun Belirtisi
PPO small-gate precision parts show gate blockage and filling fluctuation, pressure loss at the pin gate is large, and gate marks are obvious.
Neden Analizi
The high-viscosity PPO melt has great resistance passing through the small pin gate; an undersized gate diameter aggravates shear and pressure loss; cold slugs block small-bore gates; process fluctuation amplifies gate sensitivity.
Çözüm
①Appropriately enlarge the pin gate diameter; ②finely control the gate area temperature to prevent premature freezing; ③optimize the injection speed profile; ④switch to a fan gate or flat gate if necessary.
Temel Çıkarım
PPO pin gates must have enlarged diameters as industry experience; small gates and high viscosity are a natural contradiction; re-evaluating the gate form is often more thorough.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PPO; pin gate; blockage; gate diameter; shear; pressure loss