5 görüntüleme
PP Cold Slug Mark
Sorun Belirtisi
【Problem Phenomenon】Cold slug marks on PP surface, front section disorder
Neden Analizi
Nozzle temperature is low or cold slug well is insufficient; cold material at the front enters the cavity; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Çözüm
Match nozzle temperature with the front section; enlarge the cold slug well; increase injection speed; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Temel Çıkarım
For PP cold slug marks check nozzle and cold slug well; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!