Material Drying
5 görüntüleme
PSU Melt Residence and Preheating Stability
Sorun Belirtisi
[Problem Phenomenon] PSU continues molding after production interruption; product stability fluctuates
Neden Analizi
Long-time high-temperature residence affects PSU melt decomposition stability; appropriate pretreatment (maintaining dryness, avoiding long-time high-temperature retention, brief preheating before injection) can maintain stability
Çözüm
Manage production interruptions by residence time; empty when exceeding the limit; briefly preheat the melt before restart; establish standard operations for shutdown and restart; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
PSU residence time must be managed; interruption and restart follow standard operations to ensure stability; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence; Include this case in the defect archive as a reference for troubleshooting similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!