Material Drying
6 مشاهدة
PSU Melt Residence and Preheating Stability
ظاهرة المشكلة
[Problem Phenomenon] PSU continues molding after production interruption; product stability fluctuates
تحليل الأسباب
Long-time high-temperature residence affects PSU melt decomposition stability; appropriate pretreatment (maintaining dryness, avoiding long-time high-temperature retention, brief preheating before injection) can maintain stability
الحل
Manage production interruptions by residence time; empty when exceeding the limit; briefly preheat the melt before restart; establish standard operations for shutdown and restart; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
PSU residence time must be managed; interruption and restart follow standard operations to ensure stability; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence; Include this case in the defect archive as a reference for troubleshooting similar problems in the future
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!