Molds & Tooling 5 görüntüleme

TPE poor demolding

Sorun Belirtisi
Soft TPE products stick to the mold during demolding
Neden Analizi
Soft TPE has strong adhesion to the mold surface; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
Çözüm
Take the lower limit of mold temperature; release agent; increase the draft; balanced ejection; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Temel Çıkarım
Anti-sticking design for soft TPE demolding; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
TPEdemoldingmold stickingdraft