Molds & Tooling 5 görüntüleme

EAA internal shrinkage voids

Sorun Belirtisi
Shrinkage voids of 0.5-2mm diameter in the center of thick-wall EAA products
Neden Analizi
After cooling of thick-wall areas the interior shrinks but the surface has solidified, unable to feed material; holding time insufficient, gate freezes too early
Çözüm
1) Extend holding time until the gate is completely frozen; 2) Increase gate size to delay freezing; 3) Product design to reduce wall thickness difference
Temel Çıkarım
Shrinkage voids are caused by thick-wall shrinkage and insufficient holding; extending holding is the key
EAAshrinkage voidthick wallholding timegate freezing