EEA Poor Surface Gloss

Sorun Belirtisi
EEA product surface gloss <60%, below the 80% requirement, dull appearance
Neden Analizi
Mold surface roughness Ra>0.4μm; EEA crystallinity is high, surface microcrystals scatter light; improper cooling rate
Çözüm
1) Polish the mold to Ra<0.1μm mirror finish; 2) Increase mold temperature to delay crystallization and reduce scattering; 3) Add nucleating agent to control crystal size
Temel Çıkarım
Poor gloss is caused by mold roughness and crystallization scattering; polishing the mold and controlling crystallization are key
EEA gloss mold polishing crystallization scattering nucleating agent