Extrusion & Post
11 görüntüleme
EEA Surface Snakeskin Pattern
Sorun Belirtisi
Snakeskin-like irregular texture on the surface of EEA extruded products
Neden Analizi
Extrusion temperature low, melt elastic recovery uneven; die temperature distribution uneven
Çözüm
1) Increase extrusion temperature to the processing temperature range; 2) Uniformize die temperature within ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Temel Çıkarım
Snakeskin pattern is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed are key
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!