Extrusion & Post
14 visualizaciones
EEA Surface Snakeskin Pattern
Fenómeno del problema
Snakeskin-like irregular texture on the surface of EEA extruded products
Análisis de la causa
Extrusion temperature low, melt elastic recovery uneven; die temperature distribution uneven
Solución
1) Increase extrusion temperature to the processing temperature range; 2) Uniformize die temperature within ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Conclusión clave
Snakeskin pattern is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed are key
¿Le ha resultado útil?
0 personas encontraron esto útil