Extrusion & Post 11 görüntüleme

EMA Delamination When Blended with Incompatible Resins

Sorun Belirtisi
When EMA is blended with polar resins such as PA/ABS, the extrudate completely delaminates, mechanical properties extremely poor
Neden Analizi
The polarity difference between EMA and polar resins is large, compatibility is zero, interfacial adhesion extremely low, no compatibilizer used
Çözüm
1) Use EMA grafted compatibilizer EMA-g-MAH 2-5wt%; 2) Add 1-2wt% epoxy compatibilizer; 3) EMA addition <10wt% to keep the other resin as the continuous phase; 4) Twin-screw high-shear blending to disperse EMA <0.3μm
Temel Çıkarım
Blending with large polarity differences requires reactive compatibilizer to form chemical bonding at the interface to solve it
EMA blend delamination polarity difference EMA-g-MAH reactive compatibilization interfacial bonding