Extrusion & Post
11 görüntüleme
Insufficient EMA transparency
Sorun Belirtisi
EMA film haze >20%, below the 5% transparent packaging requirement
Neden Analizi
EMA methyl methacrylate content too low with crystalline region scattering; extrusion cooling rate too fast
Çözüm
1) High MMA content EMA with MMA>20% to lower crystallinity; 2) Lower cooling rate; 3) 0.3wt% nucleating agent for uniform crystallization
Temel Çıkarım
EMA transparency is affected by MMA content and crystallization scattering