Sorun Belirtisi
Shrinkage voids of 0.5-2mm diameter at the center of thick-walled EMA products
Neden Analizi
Thick wall area shrinks internally after cooling but surface already solidified preventing feeding; holding pressure time insufficient with gate freezing too early
Çözüm
1) Extend holding pressure time until gate completely freezes; 2) Increase gate size to delay freezing; 3) Product design reduces wall thickness differences
Temel Çıkarım
Shrinkage voids are caused by thick wall shrinkage and insufficient holding pressure; extending holding pressure is key
EMA shrinkage voids thick wall holding pressure time gate freezing