Extrusion & Post 11 görüntüleme

Poor thickness uniformity of EVA extruded film

Sorun Belirtisi
EVA extruded film transverse thickness deviation ±15%, exceeding the ±5% industry standard
Neden Analizi
Unreasonable die flow channel design causes uneven melt flow in wide die; EVA melt elasticity large with uneven extrusion swell; uneven air ring cooling
Çözüm
1) Adopt coat-hanger die design to ensure uniform transverse flow; 2) Fine-tune die gap within ±0.02mm; 3) Optimize air ring air volume and angle for uniform cooling; 4) Add small amount of low-elasticity resin to reduce swell difference
Temel Çıkarım
Film thickness uniformity requires coordinated optimization of die design, gap adjustment and cooling
EVA film thickness uniformity die design extrusion swell air ring cooling