Extrusion & Post 12 visualizaciones

Poor thickness uniformity of EVA extruded film

Fenómeno del problema
EVA extruded film transverse thickness deviation ±15%, exceeding the ±5% industry standard
Análisis de la causa
Unreasonable die flow channel design causes uneven melt flow in wide die; EVA melt elasticity large with uneven extrusion swell; uneven air ring cooling
Solución
1) Adopt coat-hanger die design to ensure uniform transverse flow; 2) Fine-tune die gap within ±0.02mm; 3) Optimize air ring air volume and angle for uniform cooling; 4) Add small amount of low-elasticity resin to reduce swell difference
Conclusión clave
Film thickness uniformity requires coordinated optimization of die design, gap adjustment and cooling