Delamination in PU Blending with Incompatible Resins

Sorun Belirtisi
PU blended with polar resins such as PA/ABS, extrudate completely delaminated, mechanical properties extremely poor
Neden Analizi
PU and polar resins have large polarity difference, compatibility zero, interfacial adhesion extremely low, no compatibilizer used
Çözüm
1) Use PU graft compatibilizer PU-g-MAH 2-5wt%; 2) Add epoxy-type compatibilizer 1-2wt%; 3) PU addition <10wt% to keep the other resin as the continuous phase; 4) Twin-screw high-shear blending to disperse PU <0.3μm
Temel Çıkarım
Blends with large polarity difference require reactive compatibilizer to form chemical bonding at the interface to solve it
PU blend delaminationpolarity differencePU-g-MAHreactive compatibilizationinterfacial bonding