Extrusion & Post 11 görüntüleme

Excessive Heat Shrinkage of PU Film

Sorun Belirtisi
PU film heat shrinkage at 80°C >12%, exceeding the 5% dimensional stability requirement
Neden Analizi
PU extrusion orientation released upon heating causing large shrinkage; PU coefficient of thermal expansion large; film cooling froze large amounts of orientation stress
Çözüm
1) Reduce extrusion draw ratio to decrease orientation freezing; 2) Anneal film at 60-80°C to release orientation stress; 3) Add 5-10wt% rigid resin to reduce heat shrinkage; 4) Biaxial stretching process to balance orientation
Temel Çıkarım
Film heat shrinkage is caused by orientation freezing; reducing draw ratio and annealing are key
PU filmheat shrinkageorientation releaseannealingbiaxial stretching