Extrusion & Post 13 visualizações

Excessive Heat Shrinkage of PU Film

Fenómeno do problema
PU film heat shrinkage at 80°C >12%, exceeding the 5% dimensional stability requirement
Análise das causas
PU extrusion orientation released upon heating causing large shrinkage; PU coefficient of thermal expansion large; film cooling froze large amounts of orientation stress
Solução
1) Reduce extrusion draw ratio to decrease orientation freezing; 2) Anneal film at 60-80°C to release orientation stress; 3) Add 5-10wt% rigid resin to reduce heat shrinkage; 4) Biaxial stretching process to balance orientation
Conclusão principal
Film heat shrinkage is caused by orientation freezing; reducing draw ratio and annealing are key
PU filmheat shrinkageorientation releaseannealingbiaxial stretching