Internal voids of PU

Sorun Belirtisi
1-3mm voids appear inside PU products, concentrated in the thick-wall center
Neden Analizi
Insufficient holding, thick-wall center not compacted; gas entrapped and cannot be discharged; raw material moisture vaporized
Çözüm
1) Increase holding pressure to 60-80MPa for full compaction; 2) Increase mold venting; 3) Fully dry raw material
Temel Çıkarım
Internal voids are caused by insufficient holding and gas entrapment; high-pressure holding and venting are key