Material Drying
3 Aufrufe
Internal voids of PU
Problembeschreibung
1-3mm voids appear inside PU products, concentrated in the thick-wall center
Ursachenanalyse
Insufficient holding, thick-wall center not compacted; gas entrapped and cannot be discharged; raw material moisture vaporized
Lösung
1) Increase holding pressure to 60-80MPa for full compaction; 2) Increase mold venting; 3) Fully dry raw material
Wichtigste Erkenntnis
Internal voids are caused by insufficient holding and gas entrapment; high-pressure holding and venting are key