Material Drying 5 görüntüleme

Extruded pipe inner wall surface rough

Sorun Belirtisi
The extruded pipe inner wall surface is rough, with longitudinal scratches or granular feel, especially obvious in transparent pipe inner walls
Neden Analizi
Mandrel surface rough or damaged Extrusion temperature low (below the lower limit of 170-230°C), melt fluidity insufficient Cooling too fast, inner wall not fully smoothed and sized Screw speed too fast, uneven shear Raw material contains moisture or impurities
Çözüm
Polish the mandrel surface Appropriately increase the extrusion temperature to the higher value of 170-230°C Adjust the cooling rate to avoid too fast sizing Appropriately reduce the screw speed Fully dry the raw material
Temel Çıkarım
Rough pipe inner wall requires improving the mandrel and temperature