Problem Phenomenon
The extruded pipe inner wall surface is rough, with longitudinal scratches or granular feel, especially obvious in transparent pipe inner walls
Cause Analysis
Mandrel surface rough or damaged Extrusion temperature low (below the lower limit of 170-230°C), melt fluidity insufficient Cooling too fast, inner wall not fully smoothed and sized Screw speed too fast, uneven shear Raw material contains moisture or impurities
Solution
Polish the mandrel surface Appropriately increase the extrusion temperature to the higher value of 170-230°C Adjust the cooling rate to avoid too fast sizing Appropriately reduce the screw speed Fully dry the raw material
Key Takeaway
Rough pipe inner wall requires improving the mandrel and temperature
pipe inner wallmandrelextrusion temperature