Extrusion & Post 11 görüntüleme

CEF blended with incompatible resin delaminates

Sorun Belirtisi
CEF blended with polar resins such as PA/ABS, the extrudate completely delaminates, extremely poor mechanics
Neden Analizi
CEF and polar resin polarity difference large, compatibility zero, interfacial adhesion extremely low, no compatibilizer used
Çözüm
1) Use CEF graft compatibilizer CEF-g-MAH 2-5wt%; 2) Add epoxy compatibilizer 1-2wt%; 3) CEF addition amount <10wt%, keep the other resin as continuous phase; 4) Twin-screw high-shear blending to disperse CEF <0.3μm
Temel Çıkarım
Blends with large polarity differences need reactive compatibilizers to form chemical bonding at the interface to solve
CEF blend delaminationpolarity differenceCEF-g-MAHreactive compatibilizationinterfacial bonding