Extrusion & Post 11 görüntüleme

CEF extrusion film has transverse corrugations

Sorun Belirtisi
The surface of the CEF extruded film has transverse periodic corrugations with a wavelength of 5-10mm
Neden Analizi
The haul-off roller vibrates or the speed is unstable, producing periodic stretching changes; the cooling roller is eccentric or the surface is not round, causing periodic contact pressure changes
Çözüm
1) Overhaul the haul-off roller to eliminate vibration; 2) Round the cooling roller with eccentricity <0.02mm; 3) Install a pressure stabilizing device on the extruder to eliminate pressure fluctuations; 4) Stable control of the haul-off speed ±0.5%
Temel Çıkarım
Transverse corrugations are caused by haul-off vibration and roller eccentricity; equipment overhaul and stable control are the key
CEF filmtransverse corrugationhaul-off vibrationcooling roller eccentricitypressure stabilizing device