Extrusion & Post 12 مشاهدة

CEF extrusion film has transverse corrugations

ظاهرة المشكلة
The surface of the CEF extruded film has transverse periodic corrugations with a wavelength of 5-10mm
تحليل الأسباب
The haul-off roller vibrates or the speed is unstable, producing periodic stretching changes; the cooling roller is eccentric or the surface is not round, causing periodic contact pressure changes
الحل
1) Overhaul the haul-off roller to eliminate vibration; 2) Round the cooling roller with eccentricity <0.02mm; 3) Install a pressure stabilizing device on the extruder to eliminate pressure fluctuations; 4) Stable control of the haul-off speed ±0.5%
الخلاصة الأساسية
Transverse corrugations are caused by haul-off vibration and roller eccentricity; equipment overhaul and stable control are the key