Processing Machinery 5 görüntüleme

Internal Unmelted Particles of CMC

Sorun Belirtisi
Unmelted transparent or translucent particles appear inside CMC products
Neden Analizi
Screw plasticizing capacity is insufficient and temperature is low; feeding amount is too large, exceeding plasticizing capacity; CMC melting temperature is high
Çözüm
1)Increase processing temperature to ensure full melting; 2)Reduce feeding amount to match plasticizing capacity; 3)Increase screw mixing section
Temel Çıkarım
Unmelted particles are caused by insufficient plasticizing; increasing temperature and reducing feeding are the key
CMCunmelted particlesplasticizing capacityprocessing temperaturescrew mixing