Processing Machinery 7 visualizações

Internal Unmelted Particles of CMC

Fenómeno do problema
Unmelted transparent or translucent particles appear inside CMC products
Análise das causas
Screw plasticizing capacity is insufficient and temperature is low; feeding amount is too large, exceeding plasticizing capacity; CMC melting temperature is high
Solução
1)Increase processing temperature to ensure full melting; 2)Reduce feeding amount to match plasticizing capacity; 3)Increase screw mixing section
Conclusão principal
Unmelted particles are caused by insufficient plasticizing; increasing temperature and reducing feeding are the key