DSTDP poor surface gloss

Sorun Belirtisi
DSTDP product surface gloss <60%, below the 80% requirement, dull appearance
Neden Analizi
Mold surface rough Ra>0.4μm; DSTDP crystallinity high, surface microcrystals scatter light; cooling rate improper
Çözüm
1) Polish mold to Ra<0.1μm mirror finish; 2) raise mold temperature to delay crystallization and reduce scattering; 3) add nucleating agent to control crystal size
Temel Çıkarım
Poor gloss is caused by mold roughness and crystallization scattering; polishing the mold and controlling crystallization are key