Molding Process 8 görüntüleme

DSTDP large compression set

Sorun Belirtisi
DSTDP product compression set >30%, below the 15% requirement
Neden Analizi
DSTDP elastic recovery insufficient; crosslinking degree on the low side, plastic deformation unrecoverable; density on the low side, cell walls thin, poor recovery
Çözüm
1) Increase crosslinking degree to 60-70% to reduce plastic deformation; 2) select high elastic recovery DSTDP grades; 3) add reinforcing filler
Temel Çıkarım
Large compression set is caused by insufficient crosslinking; increasing crosslinking degree is key
DSTDPcompression setcrosslinking degreeelastic recoveryreinforcing filler