Extrusion & Post
11 görüntüleme
MP film excessive heat shrinkage
Sorun Belirtisi
MP film heat shrinkage at 80°C >12%, exceeding the 5% dimensional stability requirement
Neden Analizi
MP extrusion orientation released after heating causing large shrinkage; MP thermal expansion coefficient large; film cooling froze a large amount of orientation stress
Çözüm
1) reduce extrusion draw ratio to reduce orientation freezing; 2) anneal film at 60-80°C to release orientation stress; 3) add 5-10wt% rigid resin to reduce heat shrinkage; 4) biaxial stretching process to balance orientation
Temel Çıkarım
film heat shrinkage is caused by orientation freezing; reducing draw ratio and annealing are key
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!