Extrusion & Post 14 visualizaciones

MP film excessive heat shrinkage

Fenómeno del problema
MP film heat shrinkage at 80°C >12%, exceeding the 5% dimensional stability requirement
Análisis de la causa
MP extrusion orientation released after heating causing large shrinkage; MP thermal expansion coefficient large; film cooling froze a large amount of orientation stress
Solución
1) reduce extrusion draw ratio to reduce orientation freezing; 2) anneal film at 60-80°C to release orientation stress; 3) add 5-10wt% rigid resin to reduce heat shrinkage; 4) biaxial stretching process to balance orientation
Conclusión clave
film heat shrinkage is caused by orientation freezing; reducing draw ratio and annealing are key
MP film heat shrinkage orientation release annealing biaxial stretching

¿Le ha resultado útil?

0 personas encontraron esto útil