MP performance degradation after repeated processing

Sorun Belirtisi
MP tensile strength decreases 25-30% after 3-4 recycling/reprocessing cycles
Neden Analizi
molecular chains break and degrade under repeated high-temperature shear; antioxidants exhausted in multiple processing; cumulative effect of thermo-mechanical degradation
Çözüm
1) recycled material ratio not exceeding 20-30%; 2) replenish 0.1-0.2wt% antioxidant at each re-extrusion; 3) lower processing temperature 5-10°C; 4) reduce screw speed to reduce shear
Temel Çıkarım
performance degradation from multiple processing is caused by thermo-mechanical degradation; limiting regrind and replenishing antioxidants are key
MP recycling performance degradation antioxidant replenishment thermal degradation shear degradation