Material Analysis 12 görüntüleme

MP low elongation at break

Sorun Belirtisi
MP product elongation at break <100%, below the 200% requirement
Neden Analizi
MP molecular weight low, chains short, entanglement insufficient; excessive orientation, transverse elongation extremely low; excessive crosslinking limits chain slippage
Çözüm
1) select high molecular weight MP to increase entanglement density; 2) reduce orientation, lower injection speed; 3) control crosslinking degree to avoid excess
Temel Çıkarım
low elongation at break is caused by low molecular weight and orientation; selecting high MW and reducing orientation are key
MP elongation at break molecular weight orientation control crosslinking degree