MP low elongation at break

Fenómeno del problema
MP product elongation at break <100%, below the 200% requirement
Análisis de la causa
MP molecular weight low, chains short, entanglement insufficient; excessive orientation, transverse elongation extremely low; excessive crosslinking limits chain slippage
Solución
1) select high molecular weight MP to increase entanglement density; 2) reduce orientation, lower injection speed; 3) control crosslinking degree to avoid excess
Conclusión clave
low elongation at break is caused by low molecular weight and orientation; selecting high MW and reducing orientation are key
MP elongation at break molecular weight orientation control crosslinking degree