Production & Quality 5 görüntüleme

MP Internal Inclusions

Sorun Belirtisi
0.1-0.5mm inclusions inside MP products affect appearance
Neden Analizi
Impurity particles in the raw material; dust contamination in the production environment; foreign matter mixed into the recycled material
Çözüm
1) Filter the raw material with a 120-mesh screen to remove impurities; 2) Clean the production environment to control dust; 3) Strictly sort the recycled material to remove foreign matter
Temel Çıkarım
Inclusions are caused by raw material and environmental contamination; filtration and environmental control are key
MPInclusionsRaw Material FiltrationEnvironmental CleaningRecycled Material Sorting