MP Internal Inclusions
Fenómeno del problema
0.1-0.5mm inclusions inside MP products affect appearance
Análisis de la causa
Impurity particles in the raw material; dust contamination in the production environment; foreign matter mixed into the recycled material
Solución
1) Filter the raw material with a 120-mesh screen to remove impurities; 2) Clean the production environment to control dust; 3) Strictly sort the recycled material to remove foreign matter
Conclusión clave
Inclusions are caused by raw material and environmental contamination; filtration and environmental control are key