Sorun Belirtisi
Polybutadiene PBD, as an elastomer toughening modifier or HIPS component, exhibited excessive crosslinking-related abnormalities during the extrusion process.
Neden Analizi
The Mooney viscosity of PBD affects processing; improper oxidation control leads to performance deterioration.
Çözüm
According to application requirements, add anti-aging agent to systematically solve the problem.
Temel Çıkarım
The core of PBD processing lies in structure control.