Volver a Problema y solución
Extrusion & Post 14 visualizaciones

Optimization of the excessive crosslinking problem of PBD in extrusion

Fenómeno del problema
Polybutadiene PBD, as an elastomer toughening modifier or HIPS component, exhibited excessive crosslinking-related abnormalities during the extrusion process.
Análisis de la causa
The Mooney viscosity of PBD affects processing; improper oxidation control leads to performance deterioration.
Solución
According to application requirements, add anti-aging agent to systematically solve the problem.
Conclusión clave
The core of PBD processing lies in structure control.